Progress recently has been slow – other stuff and illness (not Corona – just a heavy cold I think/hope) has been keeping me away from the shed.
I managed to get some hull planking done (plating maybe – as the panels are flat? – meh). The process of popping all the panels out of the sheets took a suprisingly long time. Even with a 22’x 11′ work space there isn’t really any room for stacking the sheets flat so i made an upright stand thing that holds the sheets on their 4′ edges, this means that to get to the back of the pile i have to take off all the sheets in front and stack them separately, rather than be able to slide them out sideways. Anyway, after a couple of hours of shed time I had all the 18 panels and corresponding butt blocks cut out.
I thought i had enough clamps to position all 6 topside panels on the boat to check for fairness and symmetry of the structure, but ran out well short of even one side of the boat. A quick trip to the Foolstation and i picked up some giant clothespeg clamps that have proved to be worth every penny. At a measly 87 pence each these are by far one of the best purchases i have ever made at that slightly dubious tool vendor. (to be fair, their stock availability is usually amazing and they’ve got me out of a few scrapes in the past, its just that the quailty of the tools they sell is usually second only from the bottom of the heap to the total mixed bag that is Amazon’s selection).
The dry fit went well, with some minor adjustments to the bevelling with the sander. I then screwed the bottom and top edges of the panel to the stringers where i could see what i was screwing into. Once attached i drew around all the internal items touching the panel so i knew where to add additional holes for the bits that i couldn’t see. The panel was then taken off, and the holes added to the panel on the bench (or rather the random gate-legged table i seem to have inherited with the workspace). Then it was re-attached to the structure, using the originally drilled screw holes and using the holes just drilled on the bench holes were rebored through the stringers and frames in the areas that i couldn’t see previously and the countersink added on the outside. The end result is a panel with the areas that require glue to be applied drawn on, and the screw holes all pre located accurately, meaning the jobs that are required when gluing are limited to simply doing the saturation coat on both stringers and frames and the panel itself, adding the 406 filler then overcoating with this adhesive mix on the panel, offering up and screwing down, using the pre-drilled screw holes to locate it precisely – in this way i was able to do 6 panels per session in the shed which equals efficiency with the glue, and also time.
When doing the bottom panels I realised that I hadn’t added the stiffener piece #6 (i think it was) to the slot in the bunk sides before gluing on the stringers… so, given i couldn’t move the stringers or the bunk sides i was left with only one option to add it back in, and that was to cut a bigger slot in the bunk side (about 20mm long) to slide it into place. I’ll fill this once the hull is turned. It could have been a lot worse, so happy that so far this is the only fail in my planning…
Once i’d glued these panels on i reviewed the B&B video and they actually recommend doing the topsides planking, then the chine, then the bottom… slightly panicking that i’d made a huge balls up by doing topsides and bottom first, i did some quick checks and i’m going to end up with the same result in the end. I’ll just be bevelling the bottom plank to accept the chine plank, whereas the B&B version involved trimming the chine plank to meet the bottom plank – which might be a bit easier. I’m 99% sure there is enough material on the chine plank to do this… that 1% is still a bit worrying though.
In other news – i’ve moved to 100% West System products for laminating and gluing. The couple of issues i had with the PEC resin was probably user error, but i’m not going to risk anything else for now. I’ll use it up on the interior coating stage. I’ve used West resins a fair amount previously and they have literally never failed, even in my incapable hands. The resin seems to be really fault-tolerant given i accidentally mixed in about 30% more hardener than necessary to one batch of resin and it still cured fine… Not that i want to repeat that.
I use a measurement of resin to hardener by weight all the time, the pumps always appear to be inaccurate, especially on small quantities such as in gluing jobs. Keeping the scales in a clear zip lock bag at all times is working wonders for their service life…
I also bought a fair amount of 406 filler for gluing purposes, the website had a disproportionately small price leap from the medium bucket of filler to the large one. But i’m pretty sure i’ve now got enough for a number of boat builds…